Pewter tableware has been cast since antiquity; Roman and medieval households ate from pewter plates and tankards for centuries.
Modern pewter is typically 91-98% tin hardened with antimony and copper, having abandoned the lead of historical formulations.
Its low melting point near 230 °C allows casting in silicone or plaster molds, keeping it popular for figurines, tankards, and jewelry.
Specifications & Metrics
DENSITY:
7.30 g/cm³
YIELD STRENGTH:
23 MPa
HARDNESS:
8 HB
Related
Tin (Sn)
Antimony (Sb)
The Bronze Age
More Alloys
7075 Aluminum Alloy
Titanium Grade 5 (Ti-6Al-4V)
Nitinol 55
Inconel 718
Monel 400
Nichrome 80/20
Sterling Silver (925)
Directory
Alloys Registry
Chemistry Hub
Teahann Knowledge Base
Annunaki
Architecture
Astronomy
Botany
Chemistry
Cybersecurity
Harry Potter
History
Human
Linguistics
Music
Mythology
Philosophy
Physics
Web APIs